Understanding Dry Film Thickness

Dry film thickness (DFT) is how thick the coating is after it has dried. It is one of the most important numbers on a data sheet.

Application · 2 min read

Key points

  • DFT is measured in microns (1 micron = 0.001 mm)
  • Too thin gives weak protection; too thick can cause problems
  • On site, you check the wet film to reach the right dry thickness
  • Always use the DFT range on the data sheet

What DFT means

When paint goes on, part of it is solvent or water, and that evaporates as it dries. What is left is the dry film. Its thickness is the DFT, measured in microns. A human hair is about 70 microns thick, so a coat may be only a little thicker than a hair.

Why it matters

  • Too thin: weak spots and a shorter life
  • Too thick: it can crack, run, or stay soft underneath
  • Corners, edges and welds tend to get less paint and may need an extra coat by brush

A picture of thin, right and too thick

Press Next to see what happens when a coating is too thin, the right thickness, or too thick.

TOO THIN: WEAK SPOTS, RUST CAN GET THROUGHRIGHT THICKNESS: AS SHOWN ON THE DATA SHEETTOO THICK: CAN CRACK, SAG OR STAY SOFT

From dry thickness to wet thickness

The data sheet gives the "volume solids": the share of the wet paint that stays as dry film. To find how thick to paint it wet: wet thickness = DFT ÷ volume solids. To estimate coverage: square metres per litre = volume solids % × 10 ÷ DFT in microns. Real coverage is lower, because some paint is lost and surfaces are rough.

Try it: wet film and coverage calculator

Wet film 167 µm
Dry film 100 µm
6.0Theoretical coverage, m² per litre
–Solvent / water that evaporates

Illustrative example only, with sample numbers. Use the volume solids and DFT range from the technical data sheet of your product. Real coverage is lower than theoretical.

How DFT is measured

While painting, a small comb or gauge checks the wet film. After it dries, an electronic gauge measures the dry film on steel. Standards such as ISO 2808 and ISO 19840 explain how, and how many readings to take.

DFT in IMPREUS data

When a data sheet gives a figure, it is shown on the product page. For example, the data sheet for IMPREUS High Performance Self-Priming Finish Coat reports a pass in 500 hours of salt-spray testing (ASTM B117) at a dry film thickness of 80 to 110 microns. Always use the DFT on the data sheet for your product.

Ask a question about this topic

Not sure how this applies to your asset? Send a short question and our technical team will reply by email.

This article is general guidance. Always follow the surface preparation, mixing, application and safety information on the product's approved technical data sheet. Standards are listed for reference.

References

  • ISO 2808: Paints and varnishes, determination of film thickness
  • ISO 19840: Corrosion protection of steel structures, measurement of dry film thickness on rough surfaces
  • ASTM B117: Standard practice for operating salt spray (fog) apparatus
Technical consultation