Key points
- Flash rust forms fast on bare, clean steel when moisture is present
- It is a warning that the surface is not ready to be coated
- Coat soon after preparation, and keep the surface dry
- Check the data sheet for how much flash rust, if any, the product can tolerate
What it is
Freshly blasted or washed steel is very reactive. In humid air, or when it is wet, a thin layer of rust can appear in minutes to hours. It looks like an even orange or brown tint and is usually very light.
Why it matters
Paint put over loose rust does not grip well. The rust layer can also hide salts and trap moisture. For most coatings the surface must be free of loose rust at the time of painting.
How to prevent it
- Plan preparation so that coating follows soon after, within the time on the data sheet.
- Keep steel temperature above the dew point (see our article on weather and painting).
- Avoid water washing before coating unless the process allows it and the surface dries fast.
- Use dehumidification in enclosed spaces such as tanks.
- Store prepared steel in dry, ventilated conditions.
What to do if it appears
Light flash rust can sometimes be brushed or swept off, depending on the coating. Heavier rust needs the preparation to be done again. Follow the surface preparation on the product data sheet.
Coatings and rust
Some products are designed to be applied on lightly rusted or minimally prepared surfaces. For example, IMPREUS Acid Resistance Mastic Epoxy Coating is described as self-priming with good performance over minimal surface preparation of steel. Always use the preparation stated for your product.
Ask a question about this topic
Not sure how this applies to your asset? Send a short question and our technical team will reply by email.
This article is general guidance. Always follow the surface preparation, mixing, application and safety information on the product's approved technical data sheet. Standards are listed for reference.
References
- ISO 8501-4: Initial surface conditions, preparation grades and flash rust grades (high-pressure water jetting)
- ISO 8502-4: Guidance on estimating the probability of condensation before paint application