Industrial Paints, Specialty Coatings & Anti-Rust Solutions
Home/Reference/Articles/Problems and fixes

Paint Blistering: Causes and Fixes

Blisters are bubbles in the paint film. They show that something got trapped under the coating, or that water is being pulled through it.

Problems and fixes · 2 min read · Updated 18 Nov 2026

Key points

  • Blisters mean trapped moisture, solvent, air or salt under the film
  • Salts left on the steel are a very common hidden cause
  • Popping a blister and repainting over it does not fix the cause
  • Find the cause first, then repair to the product data sheet

What blistering looks like

Blisters are raised bubbles, from pin-head size to several centimetres. They can be hard or soft, dry inside or filled with liquid. They often start small and spread, and they usually appear where the coating is exposed to water, sun or heat.

Common causes

  • Soluble salts (such as chlorides) left on the steel. They attract water through the film and push the coating up. This is called osmotic blistering.
  • Painting a damp or condensing surface, so moisture is sealed under the film.
  • Solvent trapped by applying a coat too thick, or recoating before the first coat has released its solvent.
  • Air trapped in a rough or porous surface during application.
  • Heat from sun on a dark surface, which makes trapped solvent or moisture expand.
  • Using a coating that is not suited to the service, for example in constant immersion.

How to find the cause

Open a few blisters. If the liquid inside tastes salty or the steel under it is rusty, salts are likely. If it is dry and the film feels soft, think of trapped solvent. Check the thickness records, the weather on the day of painting and the surface preparation that was done.

How to fix it

  • Remove the blistered coating back to sound, well-bonded paint.
  • Wash the steel and remove salts and contaminants. A final clean and dry surface is essential.
  • Prepare the surface to the level in the product data sheet.
  • Repair with the coating system on the data sheet, at the correct thickness and recoat times.

How to prevent it

Control the weather (see the dew point article), clean off salts before coating, apply at the thickness on the data sheet and respect the recoat window. For harsh or wet service, choose a system made for that service.

Ask a question about this topic

Not sure how this applies to your asset? Send a short question and our technical team will reply by email.

This article is general guidance. Always follow the surface preparation, mixing, application and safety information on the product's approved technical data sheet. Standards are listed for reference.

References

  • ISO 4628-2: Evaluation of degradation of coatings, assessment of degree of blistering
  • ISO 8502-9: Field method for the conductometric determination of water-soluble salts
  • ASTM D714: Evaluating degree of blistering of paints
Technical consultation

Not sure which coating is right?

Tell us about your asset, surface condition and operating environment. Our technical team will help you identify a suitable solution.

Chat on WhatsApp