Cracks in a coating let water reach the surface below. They come from stress that the film cannot absorb: too much thickness, ageing, movement or heat.

Problems and fixes · 2 min read · Updated 18 Nov 2026

Key points

  • Cracking is a failure of the film under stress
  • Over-thick coats and ageing are common causes
  • Movement and temperature swings in the substrate add stress
  • Light surface cracking is different from cracks that go through the film

Types of cracking

  • Checking: fine, shallow cracks in the top layer.
  • Cracking: cracks that run through a coat.
  • Mud cracking: a network like dried mud, often where a coat was applied far too thick.
  • Alligatoring: wide, deep cracks with a scaly look, often when a hard coat sits on a softer, flexible one.

Common causes

  • A coat applied thicker than the data sheet allows, so the surface hardens before the inside.
  • Ageing and weathering, as the binder loses flexibility.
  • A hard topcoat over a soft or flexible coat, so they move differently.
  • Movement of the substrate, thermal expansion and vibration.
  • Wrong recoat timing between coats.

How to deal with it

  • Find the depth. Light surface checking can sometimes be cleaned and recoated.
  • Where cracks reach the steel or the primer, remove the affected coating back to sound material.
  • Repair with a compatible system at the correct thickness.

How to prevent it

Measure and control the thickness (see our article on dry film thickness), keep to the recoat intervals, use compatible coats and choose a coating with suitable flexibility where the structure moves or sees big temperature swings.

Ask a question about this topic

Not sure how this applies to your asset? Send a short question and our technical team will reply by email.

This article is general guidance. Always follow the surface preparation, mixing, application and safety information on the product's approved technical data sheet. Standards are listed for reference.

References

  • ISO 4628-4: Assessment of degree of cracking
  • ASTM D661: Evaluating degree of cracking of exterior paints